Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 22.0 m²/g | 22.0 m²/g | BET |
KaMin Nucap® 100G Kaolin Clay - Surface Treated Cost effective, moderate brightness, mercapto silane treated clay for partial thermal black replacement.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl Rubber, EP.. |
|||
Specific Surface Area | 22.0 m²/g | 22.0 m²/g | BET |
KaMin Nucap® 190W Kaolin Clay - Surface Treated Reinforcing filler/extender for elastomeric systems. Nucap®190W is a high brightness treated kaolin used in white roofing membranes and white sidewalls. Silane treated clays mix in quicker and ma.. |
|||
Specific Surface Area | 22.0 m²/g | 22.0 m²/g | BET |
KaMin Nucap® 290W Kaolin Clay - Surface Treated Reinforcing filler/extender for elastomeric systems. Nucap®290W is a high brightness kaolin with the highest level of surface treatment to impart the best mechanical properties and water resistan.. |
|||
Specific Surface Area | 22.0 m²/g | 22.0 m²/g | BET |
KaMin Nulok® 390 Kaolin Clay - Surface Treated High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R.. |
|||
Specific Surface Area | 22.0 m²/g | 22.0 m²/g | BET |
KaMin Polygloss® 90 Kaolin Clay - Ultrafine, high brightness Ultrafine, highly pulverized, premium brightness kaolin for extending high gloss solvent and water-based coatings.Industry: Paint & Coatings, Rubber & Plastic, InkUses: Architectural Coatings, Indus.. |