Polymer Property : Specific Surface Area = 38 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 38 m²/g
38 m²/g
Statistical thickness surface area; ASTM D 6556
Orion Engineered Carbons PUREX® HS 40 Carbon Black
Carbon black grade for manufacture of mechanical rubber goods such as extruded profiles and sealsInformation provided by Orion Engineered Carbons.