Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 48 m²/g | 48 m²/g | Statistical thickness surface area; ASTM D 6556 |
Orion Engineered Carbons PUREX® HS 55 Carbon Black Carbon black grade for manufacture of mechanical rubber goods such as extruded profiles and sealsInformation provided by Orion Engineered Carbons. |
|||
Specific Surface Area | 48 m²/g | 48 m²/g | |
Zircar Ceramics NKO Castertip Main stay "low mass hard tip" used on all makes of continuous thin strip aluminum casting equipment. NKO is a rigid combination of refractory ceramic fiber and inorganic binders. Information provid.. |