Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | >= 500 m²/g | >= 500 m²/g | BET |
Nanocyl NANOCYL™ NC1101 Single-Wall Isolated and Bundled Carbon Nanotubes - Research grade NANOCYL™ NC1000 series single-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 70% ca.. |
|||
Specific Surface Area | >= 500 m²/g | >= 500 m²/g | BET |
Nanocyl NANOCYL™ NC2100 Double-Wall Isolated and Bundled Carbon Nanotubes - Research Grade NANOCYL™ NC2000 series double-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 90% ca.. |
|||
Specific Surface Area | >= 500 m²/g | >= 500 m²/g | BET |
Nanocyl NANOCYL™ NC2101 Double-Wall Isolated and Bundled Carbon Nanotubes - Research Grade NANOCYL™ NC2000 series double-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 90% ca.. |
|||
Specific Surface Area | >= 500 m²/g | >= 500 m²/g | BET |
NanoScale NanoActive® Titanium Dioxide NanoActive TiO2 is produced using proprietary processes to obtain high specific surface area (over 500 m²/g), high porosity, weakly aggregated, amorphous material possessing adsorption capacity and.. |
|||
Specific Surface Area | 500 m²/g | 500 m²/g | |
NanoAmor 95%, OD/ID: < 8/2-5 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Specific Surface Area | 500 m²/g | 500 m²/g | |
NanoAmor 95%, OD: < 8 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Specific Surface Area | 500 m²/g | 500 m²/g | |
NanoAmor 95%, OD: < 8 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Specific Surface Area | 500 m²/g | 500 m²/g | |
NanoAmor 95%, OD/ID/L: < 8/2-5 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |