Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 3.0 - 6.0 m²/g | 3.0 - 6.0 m²/g | BET |
Nabaltec NABALOX® NO 625-31 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 3.0 - 6.0 m²/g | 3.0 - 6.0 m²/g | BET |
Magyar Aluminum ALO-DF223 Alumina Alumina for Polishing |
|||
Specific Surface Area | 3.0 - 6.0 m²/g | 3.0 - 6.0 m²/g | BET |
Magyar Aluminum ALO-Ex33 Alumina Calcined Alumina |
|||
Specific Surface Area | 3.0 - 6.0 m²/g | 3.0 - 6.0 m²/g | BET |
Magyar Aluminum ALO-P95 Alumina Alumina for Polishing |
|||
Specific Surface Area | 4.0 - 6.0 m²/g | 4.0 - 6.0 m²/g | BET |
H.C. Starck Grade B-hp Silicon Carbide, SiC High purity Beta SiC powder. Min. 99.995%.Sliding bearingsSeal ringsWear partsKiln furniture, crucibles, heating elements, burner nozzles, heat exchangersSemiconductor handling partsComponents for w.. |
|||
Specific Surface Area | 4.0 - 6.0 m²/g | 4.0 - 6.0 m²/g | BET |
H.C. Starck Grade UF 05 Silicon Carbide, SiC Alpha SiC for hot-pressing and infiltration.Sliding bearingsSeal ringsWear partsKiln furniture, crucibles, heating elements, burner nozzles, heat exchangersSemiconductor handling partsComponents for.. |