Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 10 - 75 m²/g | 10 - 75 m²/g | |
American Elements Aluminum Nitride Nanoparticles General DescriptionAluminum Nitride (AlN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Aluminum Nitride Particles are typically 10 - 100 nanometers (nm).. |
|||
Specific Surface Area | 10 - 75 m²/g | 10 - 75 m²/g | |
American Elements Boron Carbide Nanoparticles General DescriptionBoron Carbide (BC) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Boron Carbide Particles are typically 10 - 100 nanometers (nm) with s.. |
|||
Specific Surface Area | 10 - 75 m²/g | 10 - 75 m²/g | |
American Elements Boron Nitride Nanoparticles General DescriptionBoron Nitride (BN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Boron Nitride Particles are typically 10 - 100 nanometers (nm) with s.. |
|||
Specific Surface Area | 10 - 75 m²/g | 10 - 75 m²/g | |
American Elements Calcium Chloride Nanoparticles General DescriptionCalcium Chloride (CaCl) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Chloride Particles are typically 10 - 100 nanometers (nm.. |
|||
Specific Surface Area | 10 - 75 m²/g | 10 - 75 m²/g | |
American Elements Silicon Carbide Nanoparticles General DescriptionSilicon Carbide (SiC) Nanoparticles, whiskers, nanodots or nanopowder are spherical high surface area particles. Nanoscale Silicon Carbide Particles are typically 10 - 150 nanomet.. |
|||
Specific Surface Area | 10 - 75 m²/g | 10 - 75 m²/g | |
American Elements Silicon Nanotubes General DescriptionSilicon (Si) Nanotubes, Single-Walled, Double Walled and Multi-Walled are tubular ultra high surface area nanotubes. Nanoscale Silicon Nanotubes are typically 10 - 100 nanometers .. |
|||
Specific Surface Area | 25 - 75 m²/g | 25 - 75 m²/g | |
American Elements Silicon Nitride Nanoparticles General DescriptionSilicon Nitride (SiN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Silicon Nitride Particles are typically 10 - 100 nanometers (nm) w.. |
|||
Specific Surface Area | 10 - 75 m²/g | 10 - 75 m²/g | |
American Elements Titanium Nitride Nanoparticles General DescriptionTitanium Nitride (TiN) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Titanium Nitride Particles are typically 10 - 100 nanometer.. |