Physical Properties Metric English Comments
Specific Surface Area 1.00 - 9.00 m²/g
1.00 - 9.00 m²/g
Average value: 2.44 m²/g Grade Count:8
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Specific Surface Area 7.00 - 9.00 m²/g
7.00 - 9.00 m²/g
BET
KaMin Polyfil® WC Kaolin Clay - Calcined
Polyfil®WC clay is an organo-functional calcined kaolin clay used in Wire and Cable and other thermoplastic applications. It is designed to reduce water vapor transmission, yields excellent wet a..