Physical Properties Metric English Comments
Specific Surface Area 90 m²/g
90 m²/g
Statistical thickness surface area; ASTM D 6556
Orion Engineered Carbons CORAX® N 375 ASTM Carbon Black
Standard grade of furnace black in accordance with the requirements of ASTM D 1765Hard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons.
Specific Surface Area >= 90 m²/g
>= 90 m²/g
BET
NanoScale NanoActive® Calcium Oxide Plus
NanoActive CaO Plus is produced using proprietary processes to obtain high specific surface area (over 90 m²/g vs. 1-2 m²/g for standard CaO), small crystallite size material possessing high chemi..