Molecular Weight 1050 g/mol
1050 g/mol
C.O.I.M. DIEXTER® G120 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..