Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 113.2 g/mol | 113.2 g/mol | |
BASF N-Ethylpiperidine Formula: C7H13NCAS: 766-09-6Description: N-Ethylpiperidine is a colorless to yellow liquid, with an amine-like odor characteristic with this product. It is miscible with water.Synonyms: EPIP, 1-Eth.. |
|||
Molecular Weight | 113.2 g/mol | 113.2 g/mol | |
BASF N-Ethylpyrrolidone-2 (NEP) Formula: C6H11NOCAS: 2687-91-4Description: N-Ethylpyrrolidone-2 (NEP) Is a colorless to yellow liquid, with an amine like odor. It is miscible in water and soluble in other organic solvents.Synonym.. |