Physical Properties Metric English Comments
Molecular Weight 12000 g/mol
12000 g/mol
Lucite International Elvacite ® 4044 Acrylic Resin
Elvacite® 4044 is a solid bead resin is a medium molecular weight butyl methacrylate-methyl methacrylate copolymer. It is a relatively soft and flexible acrylic resin for use in manufacture of ce..
Molecular Weight 12000 g/mol
12000 g/mol
Westlake Epolene® E-25 Chemically Modified Polypropylene, Maleation Processed
Product Description: Epolene E-25 is a maleic anhydride grafted polypropylene recommended as a coupling agent for polypropylene (PP) composites and for providing slip resistance in floor finish emul..
Molecular Weight 12000 g/mol
12000 g/mol
Westlake Epolene® N-15 Nonemulsifiable - Low Molecular Weight Polypropylene Polymer
Product Description: Epolene N-15 is a low viscosity polypropylene homopolymer with a high melt point and excellent hardness. Epolene N-15 is used in color concentrates, toner compounds, and as a pi..
Molecular Weight 12000 g/mol
12000 g/mol
Westlake Epolene® N-15P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Description: Epolene N-15P is a low viscosity polypropylene homopolymer powder with a high melt point and excellent hardness. Epolene N-15P is used in color concentrates, toner compounds, and as a p..