Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 1300 g/mol | 1300 g/mol | Mn; ETM 300-83 |
ExxonMobil ESCOREZ™ 1102 (Americas) Petroleum Hydrocarbon Resin Aliphatic hydrocarbon resin which is designed for use in a varity of applicaitons.Availability: Central America, North America and South AmericaInformation provided by ExxonMobil Chemical |
|||
Molecular Weight | 1300 g/mol | 1300 g/mol | Mn; ETM 300-83 |
ExxonMobil ESCOREZ™ 1304 Petroleum Hydrocarbon Resin Premium aliphatic hydrocarbon resin which is designed to tackify a variety of adhesive polymers including EVA, metallocene polyolefines, APP, APAO, natural rubber, synthetic polyisoprene, polyisobut.. |
|||
Molecular Weight | 1300 g/mol | 1300 g/mol | Mn; ETM 300-83 |
ExxonMobil ESCOREZ™ 1315 Petroleum Hydrocarbon Resin Premium aliphatic resin with a high softening point. It is a tackifying resin designed to provide high temperature performance and cohesive strength with a variety of adhesive polymers including me.. |