Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 13500 g/mol | 13500 g/mol | |
Lucite International Elvacite ® 4400 Acrylic Resin Elvacite® 4400 is a solid methacrylate copolymer bead resin designed for use in formulating thermosetting powder coating systems for exceptionally durable films. The resin may be used as the main.. |