Physical Properties Metric English Comments
Molecular Weight 140.28 g/mol
140.28 g/mol
American Elements Silicon Nitride Nanoparticles
General DescriptionSilicon Nitride (SiN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Silicon Nitride Particles are typically 10 - 100 nanometers (nm) w..