Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 142000 g/mol | 142000 g/mol | |
Lucite International Elvacite ® 2044 Acrylic Resin Elvacite® 2044 is a high molecular weight n-butyl methacrylate polymer. Elvacite® 2044 is useful in adhesives for smooth plastic films and aluminum, and in silk screen inks. It will plasticize.. |