Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Molecular Weight = 151.99 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 151.99 g/mol
151.99 g/mol
MV Labs CR800 Cr2O3 Chromium(III) oxide
Information provided by MV Laboratories.
Molecular Weight 151.99 g/mol
151.99 g/mol
American Elements Chromium Oxide Nanopowder
General DescriptionChromium Oxide (CrO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Chromium Oxide Particles are typically 10-30 nanometers..