Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 157.25 g/mol | 157.25 g/mol | |
Suqian Unitechem 2,2,6,6-tetramethyl-4-piperidinol Chemical Name: 2,2,6,6-tetramethyl-4-piperidinolCAS NO.: 2403-88-5Molecular Formula: C9H19NOUses: It is an important intermediate of hindered amine light stabilizer and synthetic hindered amine ligh.. |
|||
Molecular Weight | 157.25 g/mol | 157.25 g/mol | |
American Elements Gadolinium Nanoparticles General DescriptionGadolinium (Gd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Gadolinium Particles are typically 10 - 45 nanometers (nm) with sp.. |