Molecular Weight 165.84 g/mol
165.84 g/mol
Indium Corp. In(OH)3 Fine Indium Hydroxide
Indium Acetate is a white powder. Fine Powder Form: Primary particles range from 0.1 to 1.0 microns in size. they range in shape from spherical to elliptical to cylindrical. Agglomerates can be ..