Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 168.93 g/mol | 168.93 g/mol | |
American Elements Thulium Nanoparticles General DescriptionThulium (Tm) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Thulium Particles are typically 25 - 100 nanometers (nm) with specifi.. |