Physical Properties Metric English Comments
Molecular Weight 195.08 g/mol
195.08 g/mol
American Elements Platinum Nanoparticles
General DescriptionPlatinum (Pt) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Platinum Particles are typically 20 - 100 nanometers (nm) with..