Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 231000 - 262000 g/mol | 231000 - 262000 g/mol | Average value: 250000 g/mol Grade Count:3 |
Overview of materials for Polycarbonate-Urethane This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr.. |