Polymer Property : Molecular Weight = 25.94 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 25.94 g/mol
25.94 g/mol
Mateck Lithium Fluoride (LiF)
Optical crystals