Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 314.5 g/mol | 314.5 g/mol | |
BorsodChem ONGRONOX INP 75 D peroxide-type initiator Chemical name: Bis-(3,5,5-trimethyl-hexanoyl)-peroxide, or Di-isononanoyl-peroxide.Mol. wt: 314.50 g/mol.Active oxygen content: 5.09 %.Deflegmation material: isododecane.Major decomposition products.. |