Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 317 g/mol | 317 g/mol | |
LG Chemical DOA Plasticizer Features: LG DOA is an aliphatic plasticizer and used to keep softness of product under cold water.Application: Wrap for food package, synthetic leather, sheet, hose, gasketInformation provided by L.. |