Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 326 g/mol | 326 g/mol | |
Oceanchem Group Triphenyl Phosphate (TPP) Cas No.: 115-86-6Features: It is useful for plastic, which is of cellulose ester radical, and it is insoluble in gas, nonflammable and it has good light stability.Plastic: Acrylonitrile, butadienest.. |