Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 34000 g/mol | 34000 g/mol | |
Lucite International Elvacite ® 2013 Acrylic Resin Elvacite® 2013 is a low molecular weight methyl methacrylate / n-butyl methacrylate copolymer. It is a fast – dissolving, low viscosity grade with quick solvent release for use in industrial.. |