Physical Properties Metric English Comments
Molecular Weight 35000 g/mol
35000 g/mol
Weight average M
Pearl Engineering PEPLPET F096H Film Grade Resin
Used mainly as PET films/ sheets, known as Superbright
Molecular Weight 35000 g/mol
35000 g/mol
Weight average M
Pearl Engineering PEPLPET F096HA Film Grade Resin
Used mainly as PET films/ sheets, known as bright with anti-blocking agent.
Molecular Weight 35000 g/mol
35000 g/mol
M<sub>w</sub>
Westlake Epolene® C-10 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer
Product Description: Epolene C-10 is a branched low density polyethylene homopolymer with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color conc..