Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 373 g/mol | 373 g/mol | |
MV Labs DY800 Dy2O3 Dysprosium oxide Information provided by MV Laboratories. |
|||
Molecular Weight | 373 g/mol | 373 g/mol | |
MV Labs DY810 Dy2O3 Dysprosium oxide Information provided by MV Laboratories. |
|||
Molecular Weight | 373 g/mol | 373 g/mol | |
American Elements Dysprosium Oxide Nanopowder General DescriptionDysprosium (DyO) Oxide Nanopowder or Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Oxide Particles are typically 10 -.. |