Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 382.56 g/mol | 382.56 g/mol | |
American Elements Erbium Nanoparticles General DescriptionErbium (Er) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Erbium Particles are typically 10 - 80 nanometers (nm) with specific s.. |
|||
Molecular Weight | 382.56 g/mol | 382.56 g/mol | |
American Elements Erbium Oxide Nanopowder General DescriptionER-MITE powders and dispersions are inorganic erbium-oxide nanoparticles. ER-MITE-A products are uncoated and hydrophilic. ER-MITE-O products are coated with an organic silane (1-.. |