Polymer Property : Molecular Weight = 45000 g/mol
Polymer Property :
Molecular Weight =
45000 g/mol
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Molecular Weight
>=
45000
g/mol
>=
45000
g/mol
Sichuan Deyang Haton® hc Polyphenylene Sulfide Resin
Fiber gradeInformation provided by Sichuan Deyang Chemical Co., LTD