Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 47600 g/mol | 47600 g/mol | Mw; SABIC Method |
SABIC Innovative Plastics PPO 630 PPO (Asia Pacific) PPO* 630 resin is a medium molecular weight polymer based on Polyphenylene Ether (PPE). PPO* is intended for use as an additive or a building block in a variety of thermoplastics and thermoplastic e.. |
|||
Molecular Weight | 47600 g/mol | 47600 g/mol | Mw; SABIC Method |
SABIC Innovative Plastics PPO 630 PPO PPO* 630 resin is a medium molecular weight polymer based on Polyphenylene Ether (PPE). PPO* is intended for use as an additive or a building block in a variety of thermoplastics and thermoplastic e.. |
|||
Molecular Weight | 47600 g/mol | 47600 g/mol | Mw; SABIC Method |
SABIC Innovative Plastics PPO 630 PPO (Europe-Africa-Middle East) PPO* 630 resin is a medium molecular weight polymer based on Polyphenylene Ether (PPE). PPO* is intended for use as an additive or a building block in a variety of thermoplastics and thermoplastic e.. |