Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 512.599 g/mol | 512.599 g/mol | |
Esstech X-950-0000 BisGMA Resin, C29H36O8 Bisphenol A Glycidyl Methacrylate or bis-GMA is a high viscosity resin that has been used in dental formulations for years. Our BisGMA is manufactured with low levels of BPA or bisphenol A and low c.. |