Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 55.26 g/mol | 55.26 g/mol | |
American Elements Boron Carbide Nanoparticles General DescriptionBoron Carbide (BC) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Boron Carbide Particles are typically 10 - 100 nanometers (nm) with s.. |