Physical Properties Metric English Comments
Molecular Weight 6.00e+8 - 7.20e+8 g/mol
6.00e+8 - 7.20e+8 g/mol
Silikony Polskie Polimer MV 0.07 Methylvinylsilicone Gum
POLIMER MV is the main starting material for production of HTV silicone rubber. Methylvinylsilicone gum should be compounded with crosslinking agents (peroxides), fillers and other additives. Methyl..