Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 659 g/mol | 659 g/mol | |
Hong Kun Group UV 360 UV Absorber UV360 areas of application include polyolefins (PP, PE), olefin copolymers such as EVA as well as blends of polypropylene with elastomers. In addition UV360 is highly effective in polyacetals, polya.. |
|||