Physical Properties | Metric | English | Comments |
---|---|---|---|
Slip Level | 1050 ppm | 1050 ppm | |
ExxonMobil LDPE LD 151GZ Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |