Physical Properties | Metric | English | Comments |
---|---|---|---|
Slip Level | 1600 ppm | 1600 ppm | |
ExxonMobil LD 145.PX Packaging Resin
(discontinued **) LD 145.PX resin is a homopolymer cast film resin offering good clarity and toughness. Applications include Bread bags and other Food Packaging.Information provided by ExxonMobil Chemical |
|||
Slip Level | 1600 ppm | 1600 ppm | |
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |