Physical Properties | Metric | English | Comments |
---|---|---|---|
Slip Level | 850 ppm | 850 ppm | |
ExxonMobil LL 1001x72 Blown Film Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Slip Level | 850 ppm | 850 ppm | |
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Slip Level | 850 ppm | 850 ppm | |
ExxonMobil NTX™ NTX 150 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Slip Level | 850 ppm | 850 ppm | |
Dow DOWLEX™ 2071D Linear Low Density Polyethylene Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |