Polymer Property : Antiblock Level = 7850 ppm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Antiblock Level 7850 ppm
7850 ppm
Bapolene® 152F Polyethylene Film Grade
Bapolene 152F is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products...