Physical Properties Metric English Comments
Base Resin Density 0.961 g/cc
0.0347 lb/in³
ASTM D1505
Lotte Chemical Titan TITANZEX® HI1100 High density polyethylene
HI1100 is a non UV stabilised high density polyethylene for injection molding. HI1100 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 ..