Polymer Property : Base Resin Melt Index = 0.70 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Base Resin Melt Index 0.70 g/10 min
0.70 g/10 min
ASTM D1238
Lotte Chemical Titan TITANEX® LF0754 Linear low density polyethylene Hexene-1 resin  (discontinued **)
LF0754 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant agent. This product is used for blown film extrusion which offers outstanding toughness, extrudabilit..