Base Resin Melt Index 2.00 - 20.0 g/10 min
2.00 - 20.0 g/10 min
Average value: 7.00 g/10 min Grade Count:8
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..