Physical Properties Metric English Comments
Base Resin Melt Index 1.20 - 45.0 g/10 min

@Temperature 230 - 230 °C
1.20 - 45.0 g/10 min

@Temperature 446 - 446 °F
Average value: 16.4 g/10 min Grade Count:23
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..