Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR, Bottle | 15.5 hour @Temperature 50.0 °C |
15.5 hour @Temperature 122 °F |
BP 13C/25 |
SIDPEC EGYPTENE® HD 5402 EA HDPE Pipe Grade Applications:Ducting pipeDrainage PipeNon-pressure pipeInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |