Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | >= 300 hour @Temperature 50.0 - 50.0 °C |
>= 300 hour @Temperature 122 - 122 °F |
Average value: 300 hour Grade Count:3 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Environmental Stress Crack Resistance | >= 300 hour @Thickness 2.00 - 2.00 mm |
>= 300 hour @Thickness 0.0787 - 0.0787 in |
Average value: 300 hour Grade Count:3 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |