Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | >= 500 hour @Temperature 80.0 °C |
>= 500 hour @Temperature 176 °F |
with initial wall stress 4.6 MPa (on pipe samples d160 mm SDR 11) |
Kazanorgsintez PE2NT 11-9 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended to be processed into pressure p.. |
|||
Environmental Stress Crack Resistance | 500 hour @Thickness 3.17 mm, Temperature -40.0 °C |
500 hour @Thickness 0.125 in, Temperature -40.0 °F |
10% Igepal; ASTM D1693 |
Diamond Polymers NPP11-0242 Polyethylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |