Polymer Property : Fiber Count = 1000 dtex
Polymer Property :
Fiber Count =
1000 dtex
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Fiber Count
1000
dtex
900
denier
1/2
3M Nextelâ„¢ AF-14 Industrial Woven Fabric 312
Information provided by 3M