Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 1310 dtex | 1180 denier | |
Shakespeare ISOray Fluoropolymer UV resistant sewing thread, diameter 0.012" Extreme UV resistant, highly transparent, fluoropolymer monofilament industrial sewing thread. Excellent chemical resistance, excellent soil release and low moisture regain. Used for sewing: Awnin.. |