Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 667 - 1330 dtex | 600 - 1200 denier | |
Technetics Group PLASTOLON™ PTFE Outdoor Fiber
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Fiber Count | 667 - 1330 dtex | 600 - 1200 denier | |
Technetics Group PLASTOLON™ PTFE Oral Care Fiber
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Fiber Count | 667 - 1330 dtex | 600 - 1200 denier | |
Technetics Group PLASTOLON™ PTFE Weaving Fiber
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |