Physical Properties | Metric | English | Comments |
---|---|---|---|
Fiber Count | 144 dtex | 130 denier | |
Shakespeare Resistat® F901 A013 Nylon 66 Monofilament Resistat F901, MERGE A013 is a .13 millimeter nylon 6,6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickn.. |
|||
Fiber Count | 144 dtex | 130 denier | |
Shakespeare WhisperTouch® Ultra Soft low luster, TEX# 14 Nylon Industrial Sewing Thread Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b.. |
|||
Fiber Count | 144 dtex | 130 denier | |
Shakespeare WonderThread® SN-38 High tenacity TEX# 14 Nylon Industrial Sewing Thread Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b.. |
|||
Fiber Count | 144 dtex | 130 denier | |
Shakespeare WonderThread® SN-40 ultra soft TEX# 14 Nylon Industrial Sewing Thread Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b.. |